Current |
Deposition Rate |
Deposition Type |
Diameter |
Deposition Efficiency (%) |
TTW Dist. |
Voltage |
Wire Feed Speed |
100% CO2 |
150 A |
1.91 kg/h (4.2 lb/h) |
1.2 mm (.045 in.) |
86 % |
28 V |
508 cm/min (200 in./min) |
210 A |
2.86 kg/h (6.3 lb/h) |
1.2 mm (.045 in.) |
86 % |
29 V |
762 cm/min (300 in./min) |
250 A |
3.86 kg/h (8.5 lb/h) |
1.2 mm (.045 in.) |
87 % |
30 V |
1016 cm/min (400 in./min) |
245 A |
3.31 kg/h (7.3 lb/h) |
1.4 mm (.052 in.) |
86 % |
28 V |
635 cm/min (250 in./min) |
310 A |
4.63 kg/h (10.2 lb/h) |
1.4 mm (.052 in.) |
85 % |
33 V |
889 cm/min (350 in./min) |
360 A |
6.03 kg/h (13.3 lb/h) |
1.4 mm (.052 in.) |
85 % |
36 V |
1143 cm/min (450 in./min) |
300 A |
4.63 kg/h (10.2 lb/h) |
1.6 mm (1/16 in.) |
87 % |
30 V |
635 cm/min (250 in./min) |
365 A |
5.58 kg/h (12.3 lb/h) |
1.6 mm (1/16 in.) |
86 % |
33 V |
762 cm/min (300 in./min) |
410 A |
6.35 kg/h (14 lb/h) |
1.6 mm (1/16 in.) |
88 % |
33 V |
889 cm/min (350 in./min) |
190 A |
2.77 kg/h (6.1 lb/h) |
1.6 mm (1/16 in.) |
87 % |
27 V |
381 cm/min (150 in./min) |
155 A |
2 kg/h (4.4 lb/h) |
1.4 mm (.052 in.) |
87 % |
25 V |
381 cm/min (150 in./min) |
290-350 A |
Full Range |
1.6 mm (1/16 in.) |
19-25.4 mm (3/4-1 in.) |
26-30 V |
559-838 cm/min (220-330 in./min) |
185-290 A |
Full Range |
1.6 mm (1/16 in.) |
15.9-25.4 mm (5/8-1 in.) |
24-28 V |
279-559 cm/min (110-220 in./min) |
280-320 A |
Full Range |
1.4 mm (.052 in.) |
19-25.4 mm (3/4-1 in.) |
26-31 V |
762-1016 cm/min (300-400 in./min) |
220-280 A |
Full Range |
1.4 mm (.052 in.) |
15.9-19 mm (5/8-3/4 in.) |
25-29 V |
508-762 cm/min (200-300 in./min) |
130-220 A |
Full Range |
1.4 mm (.052 in.) |
12.7-15.9 mm (1/2-5/8 in.) |
22-26 V |
279-508 cm/min (110-200 in./min) |
225-265 A |
Full Range |
1.2 mm (.045 in.) |
19-25.4 mm (3/4-1 in.) |
26-29 V |
965-1321 mm/min (380-520 in./min) |
200-225 A |
Full Range |
1.2 mm (.045 in.) |
12.7-19 mm (1/2-3/4 in.) |
24-27 V |
660-965 cm/min (260-380 in./min) |
130-200 A |
Full Range |
1.2 mm (.045 in.) |
9.5-12.7 mm (3/8-1/2 in.) |
22-26 V |
381-660 cm/min (150-260 in./min) |
290 A |
4.85 kg/h (10.7 lb/h) |
1.2 mm (.045 in.) |
87 % |
33 V |
1270 cm/min (500 in./min) |