Dual Shield II 100-D1

ESAB

Dual Shield II 100-D1

The following items have been added to your list


x

Dual Shield II 100-D1 is an all-position flux cored electrode specially formulated to weld quenched and tempered steels that require a postweld heat treatment using 75% Ar / 25% CO2 shielding gas. Dual Shield II 100-D1 was designed to weld oil field components made of 4130, 8630, API X-80 and similar steels.

BUY NOW


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment

Welding Process

  • FCAW (Flux Core)

Typical Charpy V-Notch Properties

Stress Relieved
Impact Value 20 ft-lb
Impact Value 27 J
Shielding Gas 75% Ar - 25% CO2
1175 °F
635 °C
8 hr
Testing Temperature -25 °F
Testing Temperature -32 °C

Typical Tensile Properties

Condition Stress Relieved As Welded
Reduction in Area 58 % 58 %
Shielding Gas 75% Ar - 25% CO2 75% Ar - 25% CO2
Tensile Strength 650 MPa (94 ksi) 705 MPa (102 ksi)
Yield Strength 585 MPa (85 ksi) 650 MPa (94 ksi)
Elongation 26 % 23 %
Testing Time 8 hr
Testing Temperature 635 degC (1175 degF)

Recommended Welding Parameters

Current TTW Dist. Voltage Wire Diameter Wire Feed Speed
75% Ar - 25% CO2
130-200 A 9.5-12.7 mm (3/8-1/2 in.) 22-26 V 1.2 mm (.045 in.) 381-660 cm/min (150-260 in./min)
200-225 A 12.7-19 mm (1/2-3/4 in.) 24-27 V 1.2 mm (.045 in.) 660-965 cm/min (260-380 in./min)
225-265 A 19-25.4 mm (3/4-1 in.) 27-29 V 1.2 mm (.045 in.) 965-1321 cm/min (380-520 in./min)
135-250 A 12.7-16 mm (1/2-5/8 in.) 22-26 V 1.4 mm (.052 in.) 279-584 cm/min (110-230 in./min)
250-295 A 16-19 mm (5/8-3/4 in.) 25-29 V 1.4 mm (.052 in.) 584-864 cm/min (230-340 in./min)
295-355 A 19-25.4 mm (3/4-1 in.) 27-31 V 1.4 mm (.052 in.) 864-1194 cm/min (340-470 in./min)
185-285 A 16-19 mm (5/8-3/4 in.) 24-28 V 1.6 mm (1/16 in.) 279-508 cm/min (110-200 in./min)
285-340 A 19-25.4 mm (3/4-1 in.) 27-30 V 1.6 mm (1/16 in.) 508-762 cm/min (200-300 in./min)
340-400 A 25.4-31.75 mm (1-1.25 in.) 28-32 V 1.6 mm (1/16 in.) 762-1067 cm/min (300-420 in./min)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Voltage Wire Feed Speed
75% Ar - 25% CO2
150 A 1.9 kg/h (4.2 lb/h) 1.2 mm (.045 in.) 86 % 28 V 508 cm/min (200 in./min)
210 A 2.8 kg/h (6.3 lb/h) 1.2 mm (.045 in.) 86 % 29 V 762 cm/min (300 in./min)
250 A 3.9 kg/h (8.5 lb/h) 1.2 mm (.045 in.) 87 % 30 V 1016 cm/min (400 in./min)
290 A 4.8 kg/h (10.7 lb/h) 1.2 mm (.045 in.) 87 % 33 V 1270 cm/min (500 in./min)
155 A 2.0 kg/h (4.4 lb/h) 1.4 mm (.052 in.) 87 % 25 V 381 cm/min (150 in./min)
245 A 3.3 kg/h (7.3 lb/h) 1.4 mm (.052 in.) 86 % 28 V 635 cm/min (250 in./min)
310 A 4.6 kg/h (10.2 lb/h) 1.4 mm (.052 in.) 85 % 33 V 889 cm/min (350 in./min)
360 A 6.0 kg/h (13.3 lb/h) 1.4 mm (.052 in.) 85 % 36 V 1143 cm/min (450 in./min)
430 A 8.0 kg/h (17.6 lb/h) 1.4 mm (.052 in.) 87 % 37 V 1524 cm/min (600 in./min)
190 A 2.8 kg/h (6.1 lb/h) 1.6 mm (1/16 in.) 87 % 27 V 38 cm/min (150 in./min)
300 A 4.6 kg/h (10.2 lb/h) 1.6 mm (1/16 in.) 87 % 30 V 35 cm/min (250 in./min)
365 A 5.5 kg/h (12.3 lb/h) 1.6 mm (1/16 in.) 86 % 33 V 762 cm/min (300 in./min)
410 A 6.3 kg/h (14.0 lb/h) 1.6 mm (1/16 in.) 88 % 33 V 889 cm/min (350 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.29 :
AWS A5.36 : E101T1-M21A4-D1
AWS A5.29 : E101T1-GM

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Mo Ni P S Si
75% Ar - 25% CO2
0.06 % 1.60 % 0.33 % 0.82 % 0.009 % 0.01 % 0.40 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield II 100-D1
245014063 FIND A DISTRIBUTOR
425014065 FIND A DISTRIBUTOR
245014311 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..