Dual Shield 9000-B3 is an all-position flux cored electrode which deposits a 2.25% Cr - 1% Mo weld metal. The analysis is very similar to Dual Shield 98 CM, except 9000-B3 is for out-of-position welding. The weld metal analysis is similar to an E9018-B3 low hydrogen electrode. Dual Shield 9000-B3 is recommended for welding 2.25% Cr - 1% Mo steels. This wire is designed for single or multiple pass welding. Shielding gas of 100% CO2 and 75% Ar - remainder CO2 may be used.

BUY NOW


Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Testing Temperature Testing TimeYield Strength
Stress Relieved20 %100% CO2739 MPa (107 ksi)690 degC (1275 degF)3 hr642 MPa (93 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Voltage Wire Feed Speed
75% Ar - 25% CO2
150 A 1.91 kg/h (4.2 lb/h) 1.2 mm (.045 in.) 86 % 28 V 508 cm/min (200 in./min)
210 A 86 kg/h (6.3 lb/h) 1.2 mm (.045 in.) 86 % 29 V 762 cm/min (300 in./min)
250 A 3.86 kg/h (8.5 lb/h) 1.2 mm (.045 in.) 87 % 30 V 1016 cm/min (400 in./min)
290 A 4.85 kg/h (10.7 lb/h) 1.2 mm (.045 in.) 87 % 33 V 1270 cm/min (500 in./min)
330 A 5.76 kg/h (12.7 lb/h) 1.2 mm (.045 in.) 87 % 34 V 1524 cm/min (600 in./min)
155 A 2 kg/h (4.4 lb/h) 1.4 mm (.052 in.) 87 % 25 V 381 cm/min (150 in./min)
245 A 3.31 kg/h (7.3 lb/h) 1.4 mm (.052 in.) 86 % 28 V 635 cm/min (250 in./min)
310 A 4.63 kg/h (10.2 lb/h) 1.4 mm (.052 in.) 85 % 33 V 889 cm/min (350 in./min)
360 A 6.03 kg/h (13.3 lb/h) 1.4 mm (.052 in.) 85 % 36 V 1143 cm/min (450 in./min)
430 A 7.98 kg/h (17.6 lb/h) 1.4 mm (.052 in.) 87 % 37 V 1524 cm/min (600 in./min)
190 A 2.77 kg/h (6.1 lb/h) 1.6 mm (1/16 in.) 87 % 27 V 38 cm/min (150 in./min)
300 A 4.63 kg/h (10.2 lb/h) 1.6 mm (1/16 in.) 87 % 30 V 35 cm/min (250 in./min)
365 A 5.58 kg/h (12.3 lb/h) 1.6 mm (1/16 in.) 86 % 33 V 762 cm/min (300 in./min)
410 A 6.35 kg/h (14 lb/h) 1.6 mm (1/16 in.) 88 % 33 V 889 cm/min (350 in./min)
450 A 7.3 kg/h (16 lb/h) 1.6 mm (1/16 in.) 87 % 33 V 1016 cm/min (400 in./min)
500 A 9.11 kg/h (20.1 lb/h) 1.6 mm (1/16 in.) 87 % 39 V 1270 cm/min (500 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.29 :
AWS A5.36 : E91T1-C1PZ-B3
AWS A5.29 : E91T1-B3C

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo P S Si
100% CO2
0.06 % 2.20 % 0.60 % 1.00 % 0.01 % 0.008 % 0.60 %
100% CO2
0.008 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 9000-B3
245006523 FIND A DISTRIBUTOR
245006523-01 FIND A DISTRIBUTOR
245006424 FIND A DISTRIBUTOR
425006525 FIND A DISTRIBUTOR
245006416-01 FIND A DISTRIBUTOR
245006515 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..