Dual Shield 8000-B2L

The following items have been added to your list


x

Dual Shield 8000-B2L is an all-position flux cored electrode for low carbon grades of 1.25% Cr - 0.5% Mo steels. It is designed for use with 75% - 90% Argon, remainder CO2 shielding gases. The weld metal analysis is similar to an E8018-B2L low Hydrogen electrode.

BUY NOW


Industries

  • Chemical Industry
  • Petrochemical
  • Pipeline

Welding Process

  • FCAW (Flux Core)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Testing Temperature Testing TimeYield Strength
Stress Relieved23 %75% Ar - 25% CO2605 MPa (87 ksi)691 degC (1275 degF)1 hr525 MPa (76 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Voltage Wire Feed Speed
190 A 2.77 kg/h (6.1 lb/h) 1.6 mm (1/16 in.) 87 % 27 V 38 cm/min (150 in./min)
300 A 4.63 kg/h (10.2 lb/h) 1.6 mm (1/16 in.) 87 % 30 V 35 cm/min (250 in./min)
365 A 5.58 kg/h (12.3 lb/h) 1.6 mm (1/16 in.) 86 % 33 V 762 cm/min (300 in./min)
410 A 6.35 kg/h (14 lb/h) 1.6 mm (1/16 in.) 88 % 33 V 889 cm/min (350 in./min)
450 A 7.3 kg/h (16 lb/h) 1.6 mm (1/16 in.) 87 % 33 V 1016 cm/min (400 in./min)
500 A 9.11 kg/h (20.1 lb/h) 1.6 mm (1/16 in.) 87 % 39 V 1270 cm/min (500 in./min)
150 A 1.91 kg/h (4.2 lb/h) 1.2 mm (.045 in.) 86 % 28 V 508 cm/min (200 in./min)
210 A 86 kg/h (6.3 lb/h) 1.2 mm (.045 in.) 86 % 29 V 762 cm/min (300 in./min)
250 A 3.86 kg/h (8.5 lb/h) 1.2 mm (.045 in.) 87 % 30 V 1016 cm/min (400 in./min)
290 A 4.85 kg/h (10.7 lb/h) 1.2 mm (.045 in.) 87 % 33 V 1270 cm/min (500 in./min)
330 A 5.76 kg/h (12.7 lb/h) 1.2 mm (.045 in.) 87 % 34 V 1524 cm/min (600 in./min)
155 A 2 kg/h (4.4 lb/h) 1.4 mm (.052 in.) 87 % 25 V 381 cm/min (150 in./min)
245 A 3.31 kg/h (7.3 lb/h) 1.4 mm (.052 in.) 86 % 28 V 635 cm/min (250 in./min)
310 A 4.63 kg/h (10.2 lb/h) 1.4 mm (.052 in.) 85 % 33 V 889 cm/min (350 in./min)
360 A 6.03 kg/h (13.3 lb/h) 1.4 mm (.052 in.) 85 % 36 V 1143 cm/min (450 in./min)
430 A 7.98 kg/h (17.6 lb/h) 1.4 mm (.052 in.) 87 % 37 V 1524 cm/min (600 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.29 :
AWS A5.36 : E81T1-M21PZ-B2L
AWS A5.29 : E81T1-B2LM

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo P S Si
75% Ar - 25% CO2
0.02 % 1.40 % 0.90 % 0.50 % 0.010 % 0.010 % 0.40 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 8000-B2L
245005632 FIND A DISTRIBUTOR
245005624 FIND A DISTRIBUTOR
245005616 FIND A DISTRIBUTOR
245005566 FIND A DISTRIBUTOR
245006531 FIND A DISTRIBUTOR
245006531-43 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..