Dual Shield 7000-A1 is an all-position flux cored electrode recommended for 0.5% Mo steels. It is used in the fabrication and erection of boilers, pressure piping and tubing and other pressure vessel applications. Shielding gas of 100% CO2 and 75% Ar, remainder CO2 may be used. The weld metal analysis is similar to an E7018-A1 low hydrogen electrode.

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Mo P S Si
0.05 % 0.90 % 0.55 % 0.01 % 0.01 % 0.60 %
0.05 % 0.90 %

Classifications

AWS A5.29 : E81T1-A1C/A1M
ASME SFA 5.29 :
ASME SFA 5.36 :
AWS A5.36 : E81T1-C1PZ-A1
AWS A5.36 : E81T1-C1AZ-A1

Typical Tensile Properties

Condition As Welded Stress Relieved
Tensile Strength 635 MPa(92 ksi) 645 MPa(93 ksi)
Yield Strength 566 MPa(82 ksi) 566 MPa(82 ksi)
Elongation 22 % 26 %
Testing Time 1 hr
Testing Temperature 620 degC(1150 degF)

Deposition Data

Current Deposition Rate Diameter Efficiency (%) TTW Dist. Voltage Wire Feed Speed
100% CO2
140 A 1.7 kg/h(3.6 lb/h) 1.2 mm(.045 in.) 77.8 % 15.9 mm(5/8 in.) 24 V 508 cm/min(200 in./min)
192 A 2.5 kg/h(5.5 lb/h) 1.2 mm(.045 in.) 79.3 % 15.9 mm(5/8 in.) 25.5 V 762 cm/min(300 in./min)
230 A 3.3 kg/h(7.4 lb/h) 1.2 mm(.045 in.) 81.8 % 19 mm(3/4 in.) 27 V 1016 cm/min(400 in./min)
275 A 4.4 kg/h(9.6 lb/h) 1.2 mm(.045 in.) 83.1 % 19 mm(3/4 in.) 28.5 V 1270 cm/min(500 in./min)
150 A 1.6 kg/h(3.6 lb/h) 1.4 mm(.052 in.) 75.8 % 19 mm(3/4 in.) 23.5 V 381 cm/min(150 in./min)
190 A 2.2 kg/h(4.9 lb/h) 1.4 mm(.052 in.) 77.8 % 19 mm(3/4 in.) 24 V 508 cm/min(200 in./min)
250 A 3.5 kg/h(7.7 lb/h) 1.4 mm(.052 in.) 81.7 % 19 mm(3/4 in.) 25.5 V 762 cm/min(300 in./min)
300 A 4.7 kg/h(10.3 lb/h) 1.4 mm(.052 in.) 82.5 % 19 mm(3/4 in.) 27 V 1016 cm/min(400 in./min)
345 A 6.0 kg/h(13.3 lb/h) 1.4 mm(.052 in.) 84.7 % 19 mm(3/4 in.) 28.5 V 1270 cm/min(500 in./min)
195 A 2.5 kg/h(5.5 lb/h) 1.6 mm(1/16 in.) 85 % 19 mm(3/4 in.) 24 V 381 cm/min(150 in./min)
290 A 4.2 kg/h(9.2 lb/h) 1.6 mm(1/16 in.) 86.5 % 19 mm(3/4 in.) 25.5 V 635 cm/min(250 in./min)
325 A 4.9 kg/h(10.9 lb/h) 1.6 mm(1/16 in.) 85.9 % 19 mm(3/4 in.) 26.5 V 762 cm/min(300 in./min)
352 A 6.0 kg/h(13.1 lb/h) 1.6 mm(1/16 in.) 88.1 % 19 mm(3/4 in.) 27 V 889 cm/min(350 in./min)
382 A 6.7 kg/h(14.7 lb/h) 1.6 mm(1/16 in.) 86.8 % 19 mm(3/4 in.) 28.5 V 1016 cm/min(400 in./min)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Dual Shield 7000-A1
DS 7000-A1 045X33#AWS 245012521 FIND A DISTRIBUTOR
DS 7000-A1 045X33#AWS 245012521-01 FIND A DISTRIBUTOR
DS 7000-A1 1/16X33#AWS 245012505-01 FIND A DISTRIBUTOR
x
x

x

Loading..