Stoody 101HC, 101HC-G, 101HC-O'

Stoody

Stoody 101HC, 101HC-G, 101HC-O

Stoody 101HC, 101HC-G, 101HC-O

Stoody 101HC is a high chromium-iron based alloy recommended for metal-to earth applications subject to severe abrasion and moderate impact and heat. 101HC develops a tight crosschecking pattern.

BUY NOW


Features

  • Very tight cross checking pattern
  • Good choice for applications involving severe metal-to-earth abrasion
  • Can be used in hot wear applications up to 900° F (482° C)


Specifications


Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
56-64 HRC

Typical Weld Metal Analysis

OtherCCrFe
2.0 %5.0 %19.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
56-64 HRC

Typical Weld Metal Analysis

OtherCCrFe
2.0 %5.0 %19.0 %BAL %

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody 101HC, 101HC-G, 101HC-O
1/16 in / 1.6 mm Stoody 101HC-O 33lb WB 11304700 FIND A DISTRIBUTOR
1/16 in / 1.6 mm Stoody 101HC-O 50lb PP 11304800 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 50lb PP 11325200 FIND A DISTRIBUTOR
1/16 in / 1.6 mm Stoody 101HC-O 10lb PS 11421000 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 33lb WB 11436300 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 10lb PS 11440300 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 110lb QP 11849200 FIND A DISTRIBUTOR
7/64 in / 2.8 mm Stoody 101HC 200lb HP 11861300 FIND A DISTRIBUTOR
7/64 in / 2.8 mm Stoody 101HC 60lb Coil 11862500 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 33lb WB 11865500 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 200lb HP 11866900 FIND A DISTRIBUTOR
7/64 in / 2.8 mm Stoody 101HC 500lb POP 11873200 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 50lb PP 11874600 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 300lb NTP 11891500 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 500lb POP 11901700 FIND A DISTRIBUTOR
.035 in / 0.9 mm Stoody 101HC-G 5lb PS 11929200 FIND A DISTRIBUTOR
.035 in / .90 mm Stoody 101HC-G 25lb PS 11933400 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..