Stoody 964 AP-G
Stoody 964 AP-G is a gas shielded flux cored general purpose hardfacing wire. Deposits from this all-position wire provide exceptional wear resisteance and high hardness. On Series 300 stainless and manganese steels, deposits are crack free. Other base metals should be preheated and post-heated appropriately. Stoody 964AP-G provides improved weldability over chromium carbide and many other tool steel welding wires. Use 964 AP-G where cross checking is undesirable.
Features
- Gas shielded flux cored
- All position
- Excellent wear resistance
- High hardness
- Crack free on Series 300 stainless and manganese steels
- Little or no cross checking
- Improved weldability over chromium carbides and tool steel welding wires
Typical Tensile Properties
Shielding Gas |
75% Ar - 25% CO2 |
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage | Wire Feed Speed |
75% Ar - 25% CO2 | |||||
140-225 A | Full Range | 1.2 mm (.045 in.) | 13-19 mm (1/2-3/4 in.) | 25-29 V | 610-1194 cm/min (240-470 in./min) |
150-280 A | Full Range | 1.6 mm (1/16 in.) | 13-19 mm (1/2-3/4 in.) | 24-30 V | 381-699 cm/min (150-275 in./min) |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
1.0 % | 8.0 % | BAL % | 6.5 % |