STOODY 121, 121-G, 121-O
Stoody 121 offers uniformly dispersed chromium carbides in a semi-austenitic matrix. Recommended for applications where abrasion is severe and impact is only moderate, Stoody 121 typically cross checks when applied and can be deposited on carbon, low alloy and manganese steels. Superior performance on a wide variety of heavy equipment and earth engaging tools.
Features
- Semi-austenitic matrix with uniformly dispersed chromium carbides
- Recommended for applications with severe abrasion and only moderate impact
- Typically cross checks upon application and not machinable
- Can be applied to carbon, low alloy and manganese steels
Typical Tensile Properties
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage |
170-200 A | Full Range | 1.2 mm (.045 in.) | 13-19 mm (1/2-3/4 in.) | 22-26 V |
205-255 A | Full Range | 1.6 mm (1/16 in.) | 13-25 mm (1/2-1 in.) | 24-28 V |
250-350 A | Full Range | 2.4 mm (3/32 in.) | 19-32 mm (3/4-1 1/4 in.) | 24-28 V |
300-400 A | Full Range | 2.8 mm (7/64 in.) | 19-32 mm (3/4-1 1/4 in.) | 24-28 V |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
3.0 % | 15.0 % | BAL % | 4.0 % |