Stoody 101HC is a high chromium-iron based alloy recommended for metal-to earth applications subject to severe abrasion and moderate impact and heat. 101HC develops a tight crosschecking pattern.

BUY NOW


Features

  • Very tight cross checking pattern
  • Good choice for applications involving severe metal-to-earth abrasion
  • Can be used in hot wear applications up to 900° F (482° C)


Typical Weld Metal Analysis %

Typical Tensile Properties

Shielding Gas
98% Ar - 2% O2

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
200-260 A Full Range 1.6 mm(1/16 in.) 13-25 mm(1/2-1 in.) 24-28 V
225-375 A Full Range 2.0 mm(5/64 in.) 13-32 mm(3/4-1 1/4 in.) 24-28 V
350-450 A Full Range 2.8 mm(7/64 in.) 32-38 mm(1 1/4-1 1/2 in.) 27-29 V
98% Ar - 2% CO2
80-185 A Full Range 0.9 mm(.035 in.) 13-16 mm(1/2-5/8 in.) 15-24 V
150-200 A Full Range 1.2 mm(.045 in.) 13-19 mm(1/2-3/4 in.) 22-26 V
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody 101HC, 101HC-G, 101HC-O
.035 in / .90 mm Stoody 101HC-G 25lb PS 11933400 FIND A DISTRIBUTOR
.035 in / 0.9 mm Stoody 101HC-G 5lb PS 11929200 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 10lb PS 11440300 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 300lb NTP 11891500 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 33lb WB 11436300 FIND A DISTRIBUTOR
.045 in / 1.2 mm Stoody 101HC-G 50lb PP 11874600 FIND A DISTRIBUTOR
1/16 in / 1.6 mm Stoody 101HC-O 10lb PS 11421000 FIND A DISTRIBUTOR
1/16 in / 1.6 mm Stoody 101HC-O 33lb WB 11304700 FIND A DISTRIBUTOR
1/16 in / 1.6 mm Stoody 101HC-O 50lb PP 11304800 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 110lb QP 11849200 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 200lb HP 11866900 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 33lb WB 11865500 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 500lb POP 11901700 FIND A DISTRIBUTOR
5/64 in / 2.0 mm Stoody 101HC-O 50lb PP 11325200 FIND A DISTRIBUTOR
7/64 in / 2.8 mm Stoody 101HC 200lb HP 11861300 FIND A DISTRIBUTOR
7/64 in / 2.8 mm Stoody 101HC 500lb POP 11873200 FIND A DISTRIBUTOR
7/64 in / 2.8 mm Stoody 101HC 60lb Coil 11862500 FIND A DISTRIBUTOR
x
x

x

Loading..