Sureweld 316L electrodes produce a concave bead with smooth ripples and a self-releasing slag. It presents an excellent wetting action and fine ripples, which minimize post weld cleaning. This characteristic is particularly useful in the food and drink industry where a smooth polished surface is required. Higher molybdenum in this product increases the resistance to pitting corrosion caused by corrosive media such as acids, sulphite, and chloride solutions. It is normally used for welding 18% Cr – 12% Ni - 2.5% Mo stainless. Ideal for welding steels Types 316 & 316L.

BUY NOW


Industries

  • Food and Beverage
  • Industrial and General Fabrication
  • Petrochemical
  • Railcars
  • Ship/Barge Building

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded30 %>490 MPa (70 ksi)>430 MPa (62 ksi)

Classifications

Classifications ASME SFA 5.4 :
AWS A5.4 : E316-16/E316L-16

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni Si
0.02 % 18.8 % 0.1 % 0.65 % 2.3 % 12 % 0.60 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 316L
N3161432C FIND A DISTRIBUTOR
N3161432U FIND A DISTRIBUTOR
N3161432P
N3161324C FIND A DISTRIBUTOR
N3161324U FIND A DISTRIBUTOR
N3161324P
N3161440C FIND A DISTRIBUTOR
N3161440P

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..