Sureweld 312 Repair

ESAB

Sureweld 312 Repair

The following items have been added to your list


x

Sureweld 312 Repair electrode produce a high tensile weld deposit and rich chemistry. As a result, it is one of the most widely used stainless steel stick electrodes , being used to weld dissimilar steels, abrasion resistant steels, high yield steels and for joining high temperature alloys to carbon or low alloy steels. It is a normal choice if you are going to weld an unknown stainless grade to another stainless or carbon steel. Sureweld 312 Repair produce a quality welding deposit, with high ductility and free of cracks and porosity. It can be used to weld Mn steels, and others high strength steels, such as hardening , armour and spring steels, and also as buffer layer for hardfacing.

BUY NOW


Industries

  • Agricultural Equipment
  • Industrial and General Fabrication
  • Steel Industry
  • Mining
  • Repair and Maintenance

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded22 %>660 MPa (95 ksi)>590 MPa (85 ksi)

Classifications

Classifications ASME SFA 5.4 :
AWS A5.4 : E312-16

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni Si
0.12 % 28.5 % 0.1 % 0.80 % 0.05 % 10 % 0.70 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 312 Repair
N3121432U FIND A DISTRIBUTOR
N3121432P
N3121324U FIND A DISTRIBUTOR
N3121324P
N3121440P

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..