Sureweld 309L electrodes produce a concave bead with smooth ripples and a self-releasing slag. For welding dissimilar carbon steel to stainless steel or to weld 22% Cr - 12% Ni stainless steels for service below about 315°C (600°F) and for the first layer when cladding.

BUY NOW


Industries

  • Industrial and General Fabrication

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded30 %>520 MPa (75 ksi)>450 MPa (65 ksi)

Classifications

Classifications ASME SFA 5.4 :
AWS A5.4 : E309-16/E309L-16

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni Si
0.03 % 23.3 % 0.1 % 0.62 % 0.1 % 13.25 % 0.70 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 309L
N3091432C FIND A DISTRIBUTOR
N3091432U FIND A DISTRIBUTOR
N3091432P
N3091324C FIND A DISTRIBUTOR
N3091324U FIND A DISTRIBUTOR
N3091324P
N3091440C FIND A DISTRIBUTOR
N3091440P

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..