Sureweld 308L

ESAB

Sureweld 308L

The following items have been added to your list


x

Sureweld 308L electrodes produce a concave bead with smooth ripples and a self-releasing slag. These electrodes are designed to weld many stainless steels including, but not limited to 301, 302, 304L & 304. It presents an excellent wetting action and fine ripples, which minimize post weld cleaning. This characteristic is particularly useful in the food and drink industry where a smooth polished surface is required.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Pressure Vessels
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded30 %>520 MPa (75 ksi)>390 MPa (57 ksi)

Classifications

Classifications ASME SFA 5.4 :
AWS A5.4 : E308-16/E308L-16

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni Si
0.02 % 18.9 % 0.1 % 0.62 % 0.1 % 9.9 % 0.85 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 308L
N3081432C FIND A DISTRIBUTOR
N3081432U FIND A DISTRIBUTOR
N3081432P
N3081324C FIND A DISTRIBUTOR
N3081324U FIND A DISTRIBUTOR
N3081324P
N3081440C FIND A DISTRIBUTOR
N3081440P

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.