OK 68.17
OK 68.17 is a coated electrode designed for the welding of stainless-steel castings of the 13Cr4NiMo type, for example. OK 68.17 can be welded in all positions apart from vertical down.
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Mn | Mo | Ni | Si | |||||||||
0.02 % | 12.0 % | 0.6 % | 0.6 % | 4.6 % | 0.4 % |
Approvals
Society | Seproz |
Grade | UNA 272580 |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Charpy V-Notch Properties
Conditional Statement | Impact Value (met) | Testing Temperature | ||
ISO | ||||
Stress relieved | 45 J(33 ft-lb) | 8 hr | 600 degC(1112 degF) | 20 degC(68 degF) |
Stress relieved | 45 J(33 ft-lb) | 8 hr | 600 degC(1112 degF) | -10 degC(14 degF) |
Stress relieved | 40 J(29.5 ft-lb) | 8 hr | 600 degC(1112 degF) | -40 degC(-40 degF) |