OK 67.43 is an austentitic, stainless steel, AC/DC electrode, which deposits a weld metal with a small amount of uniformly distributed ferrite. The tough weld metal has excellent crack resistance, even when welding steels with very poor weldability. Suitable for welding 13Mn steels and steels of this kind to other steels.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded iso
52 J (38 ft-lb) -60 degC (-76 degF)
80 J (59 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded35 %ISO630 MPa (91 ksi)440 MPa (64 ksi)

Deposition Data

Current Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal Voltage
60-80 A 46 sec 0.8 kg/h (1,8 lb/h) 2.5 x 300.0 mm (0.098 x 11,8 in.) 51 % 106 22 V
90-115 A 54 sec 1.3 kg/h (2,9 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 54 % 57 23 V
100-150 A 61 sec 1.7 kg/h (3,7 lb/h) 4.0 x 350.0 mm (5/32 x 13,8 in.) 56 % 35 23 V
130-210 A 86 sec 2.8 kg/h (6,2 lb/h) 5.0 x 450.0 mm (0.197 x 17,7 in.) 60 % 17 24 V

Classifications

Classifications EN 14700 : E Fe10
EN ISO 3581-A : E 18 8 Mn R 1 2
SFA/AWS A5.4 : (E307-16)
Werkstoffnummer : 1.4370

Approvals

Approvals CE EN 13479
DB 30.039.07
VdTÜV 06797
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic. CrNiMn
Coating Type Rutile Basic
Ferrite Content FN <5
Welding Current AC, DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn N Ni Si Si+Fe
0.08 % 18.4 % 5.4 % 0.08 % 9.1 % 0.8 % 2 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK 67.43
67432520L0 FIND A DISTRIBUTOR
67433230T0 FIND A DISTRIBUTOR
67434030G0 FIND A DISTRIBUTOR
67435040G0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..