OK 67.13
OK 67.13 is an austenitic, stainless-steel electrode for welding 25Cr20Ni steels. The weld metal resists scaling up to 1100-1150°C and does not contain any measureable ferrite. OK 67.13 can also be used for welding certain air-hardening steels such as armour plate and for welding stainless to unalloyed steel.
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Mn | Ni | Si | ||||||||||
0.12 % | 25.6 % | 1.9 % | 21.1 % | 0.6 % |
Typical Charpy V-Notch Properties
Testing Temperature | 20 degC |
Testing Temperature | 68 degF |
Shielding Gas | AWS |
Impact Value (met) | 90 J |
Impact Value (imp) | 66 ft-lb |
Conditional Statement | As welded |