ESAB

Cryoarc 316L-15

The following items have been added to your list


x

Cryoarc 316L-15 electrodes are designed to be used in cryogenic applications where impact toughness is required. Cryoarc electrodes can also be used where low magnetic permeability is required.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 35 ft-lb
Impact Value 47 J
Testing Temperature -320 °F
Testing Temperature -196 °C

Typical Tensile Properties

ConditionElongationTensile Strength
As Welded45 %552 MPa (80 ksi)

Classifications

Grade 316L-15
Name SFA/AWS A5.4

Consumable Characteristics

Alloy Type Austenitic CrNiMo
Coating Type Basic
Ferrite Content max. FN 2
Welding Current AC, DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo N Ni Si Si+Fe
0.03 % 18.0 % 2.0 % 2.2 % 0.05 % 13.6 % 0.5 % 5 %