Arcaloy 316LF5-16

ESAB

Arcaloy 316LF5-16

The following items have been added to your list


x

Arcaloy 316LF5-16 is an E316L-16 electrode where the composition has been balanced to give a weld deposit with a minimum ferrite content of 5 FN. It can be used to weld Type 304L stainless steel where the presence of molybdenum is not detrimental.

BUY NOW


Industries

  • Chemical Industry
  • Food and Beverage
  • Industrial and General Fabrication
  • Petrochemical

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded40 %570 MPa (83 ksi)450 MPa (65 ksi)

Classifications

Grade E316-16/E316L-16
Name AWS A5.4

Approvals

Approvals CWB CSA W48 E316L-16
QPL MIL-E-22200/2 MIL-316L-16
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Ferrite Mn Mo Ni Si
0.03 % 19 % 0.20 % 6 FN % 1.50 % 2.50 % 12 % 0.40 %
0.20 % 1.50 % 0.40 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy 316LF5-16
251181400 FIND A DISTRIBUTOR
251181806 FIND A DISTRIBUTOR
251183109 FIND A DISTRIBUTOR
251183315 FIND A DISTRIBUTOR
251183307 FIND A DISTRIBUTOR
251185302 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..