Arcaloy 316LF-15 is a 316L electrode designed to give a weld deposit with a minimum ferrite number of 5 FN. Carbon content is 0.04% maximum and can be used to weld Type 304L stainless steal where the presence of molybdenum is not detrimental.

BUY NOW


Industries

  • Petrochemical
  • Industrial and General Fabrication
  • Food and Beverage
  • Chemical Industry

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 81 ksi 62 ksi

Typical Weld Metal Analysis %

weld metal analysis
MnMoCuCSiFerriteNiCr
1.50 %2.40 %0.20 %0.03 %0.50 %6 FN %12 %19 %

Approvals: QPL-22200/2; MIL-316L-15
Classifications: AWS A5.4; E316-15/E316L-15

Approvals are based on factory location. Please contact ESAB for more information.


x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 81 ksi 62 ksi

Typical Weld Metal Analysis %

weld metal analysis
MnMoCuCSiFerriteNiCr
1.50 %2.40 %0.20 %0.03 %0.50 %6 FN %12 %19 %

Approvals: QPL-22200/2; MIL-316L-15
Classifications: AWS A5.4; E316-15/E316L-15

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ARCALOY 316LF5-15
AC 316LF5-15 1/8X14X10#HS 251191805 FIND A DISTRIBUTOR
AC 316LF5-15 3/32X12X10#HS 252026000 FIND A DISTRIBUTOR
AC 316LF5-15 5/32X14X10#HS 251195301 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..