ARCALOY 316L-17 PLUSARCALOY 316L-17 PLUS'


ARCALOY 316L-17 PLUS

ARCALOY 316L-17 PLUS

Arcaloy 316L-17 Plus electrodes have a heavy coating and produce a concave bead with minimal ripple. The slag is virtually self-cleaning. Molybdenum increases the resistance to pitting corrosion caused by corrosive media such as sulfuric and sulfurous acids, sulphites, chlorides and cellulose solutions. Ideal for welding Types 316 & 316L stainless steels when bead appearance is important.

BUY NOW


Specifications


Typical Tensile Properties

Elongation Tensile Strength Yield Strength
(in 2") 45 % 83 ksi 64 ksi

Welding Parameters

Flat Amps Overhead Amps Vertical Amps Wire Diameter
20-35 A 20-30 A 15-25 A 1.6 mm
30-50 A 30-40 A 25-35 A 2.0 mm
60-85 A 40-60 A 40-60 A 2.4 mm
90-120 A 60-85 A 70-80 A 1/8 in.
140-165 A 95-120 A 80-90 A 4.0 mm
180-210 A 125-150 A 100-115 A 3/16 in.
205-290 A - - 1/4 in.

Typical Weld Metal Analysis %

weld metal analysis
MnMoCuCSiNiCr
0.6 %2.5 %0.1 %0.02 %0.6 %12 %19 %

Approvals: ASME IX F No. 5; ASME II SFA A5.4; E316-17/E316L-17; AWS A5.4; E316-17/E316L-17; CWB; CSA W48 E316L-17

Approvals are based on factory location. Please contact ESAB for more information.


x

Typical Tensile Properties

Elongation Tensile Strength Yield Strength
(in 2") 45 % 83 ksi 64 ksi

Welding Parameters

Flat Amps Overhead Amps Vertical Amps Wire Diameter
20-35 A 20-30 A 15-25 A 1.6 mm
30-50 A 30-40 A 25-35 A 2.0 mm
60-85 A 40-60 A 40-60 A 2.4 mm
90-120 A 60-85 A 70-80 A 1/8 in.
140-165 A 95-120 A 80-90 A 4.0 mm
180-210 A 125-150 A 100-115 A 3/16 in.
205-290 A - - 1/4 in.

Typical Weld Metal Analysis %

weld metal analysis
MnMoCuCSiNiCr
0.6 %2.5 %0.1 %0.02 %0.6 %12 %19 %

Approvals: ASME IX F No. 5; ASME II SFA A5.4; E316-17/E316L-17; AWS A5.4; E316-17/E316L-17; CWB; CSA W48 E316L-17

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ARCALOY 316L-17 PLUS
AC 316L-17 1/8X14X10X60 251311015 FIND A DISTRIBUTOR
AC 316L-17 3/16X14X10#HS 251311031 FIND A DISTRIBUTOR
AC 316L-17 3/32X12X8#HS 251311007 FIND A DISTRIBUTOR
AC 316L-17 5/32X14X10#HS 251311023 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..