Arcaloy 316/316H-16

The following items have been added to your list


x

Arcaloy 316/316H-16 should be used in applications where Type 316 stainless steel needs improved high temperature. In some cases an E16-8-2 filler metal should be used. It can also be used to weld Type 316 stainless steel for ambient temperature service.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Petrochemical

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded40 %660 MPa (85 ksi)490 MPa (65 ksi)

Classifications

Grade E316/316H-16
Name AWS A5.4

Approvals

Approvals ABS AWS A5.4: E316/316H-16
QPL MIL-E-22200/2 MIL-316-16
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Ferrite Mn Mo Ni Si
0.05 % 19 % 0.20 % 5.5 FN % 1.60 % 2.30 % 12 % 0.40 %
0.05 % 0.20 % 0.40 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy 316/316H-16
251185674 Find a distributor
251185641 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..