ESAB

Arcaloy 309L-17 PLUS

The following items have been added to your list


x

Arcaloy 309L-17 Plus electrodes have a heavy coating and produce a concave bead with minimal ripple. The slag is virtually self-cleaning. For welding carbon steel to stainless steel for service below about 315°C (600°F) and for the first layer when cladding.

BUY NOW


Industries

  • Industrial and General Fabrication

Typical Tensile Properties

ElongationTensile Strength Yield Strength
(in 2") 37 %590 MPa (85 ksi)450 MPa (65 ksi)

Recommended Welding Parameters

Flat Amps Overhead Amps Vertical Amps Wire Diameter
60-85 A 40-60 A 35-50 A 2.4 mm (3/32 in.)
90-120 A 60-85 A 55-70 A 3.2 mm (1/8 in.)
140-165 A 95-120 A 85-100 A 4.0 mm (5/32 in.)

Approvals

Approvals ASME II SFA A5.4 E309L-17/E309-17
ASME IX F No. 5
AWS A5.4 E309L-17/E309-17
CWB E309L-17
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni Si
0.025 % 23.5 % 0.1 % 0.6 % 0.1 % 13.5 % 0.7 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy 309L-17 PLUS
258074269 Find a distributor
258074285 Find a distributor
258074251 Find a distributor