Arcaloy 309L-16
Arcaloy 309L-16 is used for welding carbon and low alloy steels to stainless steels. This can be done provided the service temperature does not exceed about 700°F (370°C). Post weld heat treatment should only be performed after due consideration.
Industries
- Industrial and General Fabrication
Welding Process
- SMAW/MMA (Stick)
Typical Tensile Properties
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 37 % | 590 MPa (85 ksi) | 450 MPa (65 ksi) |
Classifications
Classifications |
ASME II SFA A5.4 : ASME IX F No. 5 : AWS A5.4 : E309L-16/E309-16 |
Approvals
Grade | E309L-16 |
Society | CWB CSA W48 |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Cu | Ferrite | Mn | Mo | Ni | Si | |||||||
0.03 % | 23.50 % | 0.10 % | 9 FN % | 1.80 % | 0.30 % | 13.50 % | 0.45 % |