Arcaloy 309L-15 is used for welding carbon and low alloy steels to stainless steels. This can be done provided the service temperature does not exceed about 700°F (370°). Post weld heat treatment should only be taken with great care. Arcaloy 309L-15 can be used as the first layer of stainless steel on carbon or low alloy steel.

BUY NOW


Industries

  • Industrial and General Fabrication

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded45 %590 MPa (85 ksi)415 MPa (60 ksi)

Classifications

Grade E309L-15/E309-15
Name AWS A5.4

Approvals

Approvals ASME II SFA A5.4 E309L-15/E309-15
ASME IX F No. 5
AWS A5.4 E309L-15/E309-15
QPL MIL-E-22200/2 MIL-309L-15
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Ferrite Mn Mo Ni Si
0.035 % 24 % 0.1 % 9 FN % 1.8 % 0.3 % 13.5 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy 309L-15
251061800 Find a distributor
251063319 Find a distributor
251065306 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..