Arcaloy 308L-16 electrodes were developed for the welding of Type 304L stainless steels but can be used for many other stainless steels including Types 301, 302 & 304. They are used extensively for the welding of chemical plant equipment and may be used successfully for the welding of Types 321 and 347 stainless steels provided the service temperature is less than about 700°F (375°C). The basic-rutile thin coating of Arcaloy 308L-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking. Operates on AC or DC current.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Petrochemical
  • Ship/Barge Building
  • Tank and Vessel Fabrication

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded45 %520 MPa (90 ksi)460 MPa (66 ksi)

Classifications

Grade E308-16/E308L-16
Name AWS A5.4

Approvals

Approvals CWB CSA W48 E308L-16
QPL-22200/2 MIL-308L-16
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Ferrite Mn Mo Ni Si
0.03 % 20 % 0.10 % 6 FN % 1.70 % 0.10 % 10 % 0.50 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Arcaloy 308L-16
251011805
251013108 FIND A DISTRIBUTOR
251013207 FIND A DISTRIBUTOR
251013306 FIND A DISTRIBUTOR
251015301 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..