OK NiCrMo-3
Ni-based CrMoNb electrode for welding of Ni-alloys of the same or similar type as e.g. Inconel 625, for welding of 5% and 9% Ni steel. The electrode is very suitable for welding of 254 SMO, i.e. UNS S31254 steel.
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature | |||
as welded iso | ||||
70 J | 20 degC | |||
50 J | -196 degC |
Typical Tensile Properties
Condition | Elongation | Shielding Gas | Tensile Strength | Yield Strength |
As Welded | 35 % | ISO | 780 MPa | 500 MPa |
Deposition Data
Current | Deposition Rate | Diameter | Number of electrodes/kg weld metal | Voltage | kg weld metal/kg electrodes | |
55-75 A | 40 sec | 0.9 kg/h | 2.5 x 300 mm | 100 | 23 V | 0.55 |
65-100 A | 52 sec | 1.4 kg/h | 3.2 x 350 mm | 49 | 25 V | 0.56 |
80-140 A | 57 sec | 1.9 kg/h | 4.0 x 350 mm | 33 | 27 V | 0.58 |
120-170 A | 72 sec | 2.1 kg/h | 5.0 x 350 mm | 21 | 24 V | 0.58 |
Classifications
Classifications |
SFA/AWS A5.11 : ENiCrMo-3 EN ISO 14172 : E Ni 6625 (NiCr22Mo9Nb) |
Approvals
Approvals |
CE EN 13479 DNV-GL -H5 NAKS/HAKC 2.5-4.0 mm VdTÜV 12414 |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Ni-based CrMoNb |
Coating Type | Basic |
Ferrite Content | FN 0 |
Welding Current | DC+ |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Fe | Mn | Mo | Nb | Ni | Si | |||||||
0.03 % | 21.7 % | 2.0 % | 0.2 % | 9.3 % | 3.3 % | 62.8 % | 0.4 % |