OK NiCrMo-13
OK NiCrMo-13 is suitable for welding Ni base materials such as Alloy 59, Hasteloy C-276, Inconel 625 and Incoloy 825. It can also be used for welding super austenitic steels type AISI/ASTM S31254 and S32654. The weld metal provides very good resistance against pitting- and chloride ion stress corrosion cracking.
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Fe | Mn | Mo | Ni | Si | ||||||||
0.013 % | 22.6 % | 0.6 % | 0.17 % | 15.2 % | 61 % | 0.16 % |
Typical Charpy V-Notch Properties
Conditional Statement | Impact Value (met) | Testing Temperature | ||
ISO | ||||
As welded | 70 J(52 ft-lb) | -60 degC(-76 degF) | ||
AWS | ||||
As welded | -196 degC(-321 degF) | |||
ISO | ||||
As welded | 60 J(44 ft-lb) | -196 degC(-321 degF) | ||
AWS | ||||
As welded | -60 degC(-76 degF) |