OK NiCrFe-3
Nickel based electrode for welding Inconel 600 and similar Inconel alloys, cryogenic steels, martensitic to austenitic steels, dissimilar steels, heat resisting steel castings of limited weldability.
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Fe | Mn | Nb | Ni | Si | ||||||||
0.04 % | 15.6 % | 6.3 % | 6.7 % | 1.7 % | 71 % | 0.8 % |