OK Ni-1 is a stick electrode for joining commercial pure nickel in wrought and cast forms. It can also be used to join dissimilar metals such as nickel to steel, nickel to copper and copper to steel. Moreover, this electrode can be used for surfacing steel.

BUY NOW


Typical Tensile Properties

ElongationShielding GasTensile Strength Yield Strength
30 %ISO470 MPa (68 ksi)330 MPa (48 ksi)

Deposition Data

Current Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal
70-95 A 47 sec 0.8 kg/h (1,8 lb/h) 2.5 x 300.0 mm (0.098 x 11,8 in.) 55 % 96
90-135 A 56 sec 1.2 kg/h (2,6 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 55 % 53

Classifications

Classifications SFA/AWS A5.11 : ENi-1
EN ISO 14172 : E Ni 2061 (NiTi3)

Consumable Characteristics

Alloy Type Nickel-base
Coating Type Lime Basic
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
Al C Fe Mn Ni Si Ti
0.10 % 0.04 % 0.4 % 0.4 % 96 % 0.7 % 1.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Ni-1
92052520L0 FIND A DISTRIBUTOR
92053230L0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..