SUREWELD 710P

SUREWELD 710P

Sureweld 710P is an all-position cellulosic electrode that is especially suited for welding high strength pipe. It produces the consistent, deep penetration required to maintain a proper keyhole when vertical-down welding in open root pipe joints. X-ray quality joints can be produced with Sureweld 710P using flat, horizontal, overhead, vertical-up and vertical-down welding procedures. Sureweld 710P is recommended for welding API grades X46, X52, and X56 pipe. It may also be used for welding root passes in higher grade pipe in some circumstances.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Pipeline

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 81 ksi 69 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 29 ft-lb -20 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnMoCSSiNi
0.01 %0.30 %0.24 %0.10 %0.02 %0.20 %0.50 %

Approvals: Conforms to E7010-G
Classifications: ASME SFA 5.5; AWS A5.5; E7010-P1

Approvals are based on factory location. Please contact ESAB for more information.


Coating Type: High cellulose
CTOD-Tested: False
Welding Current: DC+
x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 81 ksi 69 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 29 ft-lb -20 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnMoCSSiNi
0.01 %0.30 %0.24 %0.10 %0.02 %0.20 %0.50 %

Approvals: Conforms to E7010-G
Classifications: ASME SFA 5.5; AWS A5.5; E7010-P1

Approvals are based on factory location. Please contact ESAB for more information.


Coating Type: High cellulose
CTOD-Tested: False
Welding Current: DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : SUREWELD 710P
SW 710P 5/32X14X50#HS 811070036 Buy Local
SW 710P 3/16X14X50#HS 811070044 Buy Local
SW 710P 1/8X14X50#HS 811070028 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..