Sureweld 7024 is a high speed, heavy-coated, iron powder electrode for high deposition rates on horizontal and downhand welding. Excellent operator appeal, produces equal 45 deg; fillets, thereby eliminating over welding. Excellent bead appearance and self-cleaning slag. This electrode has good weldability and superior mechanical properties. It is particularly useful in obtaining increased penetration with little or no root porosity in horizontal or positioned fillets. Sureweld 7024 is ideal for making high speed horizontal fillet and lap welds on mild and some alloy steels, such as earthmoving and construction equipment, truck bodies, ships, barges and railcars. Sureweld 7024 exceeds the AWS A5.1 elongation % and Charpy V-Notch requirements for 7024-1.

BUY NOW


Industries

  • Barges
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars

Welding Process

  • SMAW/MMA (Stick)

Typical Charpy V-Notch Properties

As Welded
Impact Value 25 ft-lb
Impact Value 34 J
Testing Temperature 0 °F
Testing Temperature -18 °C

Typical Tensile Properties

ConditionElongationReduction in AreaTensile Strength Yield Strength
As Welded26 %63 %550 MPa (81 ksi)490 MPa (71 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Optimal Amps
180-240 A 2.4 kg/h (5.3 lb/h) 4.0 mm (5/32 in.) 71.3 % 180 A
180-240 A 2.9 kg/h (6.3 lb/h) 4.0 mm (5/32 in.) 72.5 % 210 A
180-240 A 3.3 kg/h (7.2 lb/h) 4.0 mm (5/32 in.) 69.4 % 240 A
250-290 A 3.4 kg/h (7.5 lb/h) 4.8 mm (3/16 in.) 69.2 % 245 A
250-290 A 3.8 kg/h (8.3 lb/h) 4.8 mm (3/16 in.) 70.5 % 270 A
250-290 A 4.1 kg/h (9.1 lb/h) 4.8 mm (3/16 in.) 68 % 290 A
300-340 A 4.3 kg/h (9.4 lb/h) 5.6 mm (7/32 in.) 72.4 % 320 A
300-340 A 5.3 kg/h (11.6 lb/h) 5.6 mm (7/32 in.) 69.1 % 360 A
350-400 A 5.7 kg/h (12.6 lb/h) 6.4 mm (1/4 in.) 71.7 % 400 A

Classifications

Classifications ASME SFA 5.1 :
AWS A5.1 : E7024

Approvals

Approvals ABS
CWB CSA W48 E4924
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Coating Type Iron powder, titania
0
Welding Current DC+, DC- or AC

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
0.06 % 0.80 % 0.01 % 0.018 % 0.30 %
0.018 % 0.30 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 7024
812000289 FIND A DISTRIBUTOR
812000248 FIND A DISTRIBUTOR
812000263 FIND A DISTRIBUTOR
812000255 FIND A DISTRIBUTOR
812000271 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..