Sureweld 7014

ESAB

Sureweld 7014

The following items have been added to your list


x

Sureweld 7014 is an iron powder coated electrode permitting the use of higher welding currents while improving the deposition rate. High speeds and high heats can be used without undercut. Slag removal is excellent. Sureweld 7014 is widely used for welding mild steels such as ASTM A-36, A-113, A-283, A-284, A-285, A-306, A-515 and A-516. Typical applications include construction equipment, metal fixtures, automotive parts, barges and farm machinery.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationReduction in AreaTensile Strength Yield Strength
As Welded28 %64 %490 MPa (71 ksi)420 MPa (61 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%)
100-150 A 1.1 kg/h (2.4 lb/h) 3.2 mm (1/8 in.) 63.9 %
100-150 A 1.4 kg/h (3.1 lb/h) 3.2 mm (1/8 in.) 61.1 %
70-100 A 0.9 kg/h (2 lb/h) 2.4 mm (3/32 in.) 60 %
160-200 A 1.4 kg/h (3 lb/h) 4.0 mm (5/32 in.) 71.9 %
160-200 A 1.7 kg/h (3.7 lb/h) 4.0 mm (5/32 in.) 67 %

Classifications

Grade E7014
Name AWS A5.1

Consumable Characteristics

Coating Type Iron powder, titania
0
Welding Current DC+, DC- or AC

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
0.04 % 0.30 % 0.02 % 0.02 % 0.14 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 7014
812000202 FIND A DISTRIBUTOR
812000206
812000214 FIND A DISTRIBUTOR
812000176 FIND A DISTRIBUTOR
812000180
812000198 FIND A DISTRIBUTOR
812000222 FIND A DISTRIBUTOR
812000230 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..