Sureweld 6013

ESAB

Sureweld 6013

The following items have been added to your list


x

Sureweld 6013 is an all-position electrode. The arc is very stable even when low-voltage open circuit transformers are used. The power of its arc allows depositing quick welds, medium penetration, and good appearance. Sureweld 6013 minimizes the risk of trapping the slag due to its special characteristics and mineral coating. Sureweld 6013 is used on a wide array of mild steel fabrication where ease of operation and good appearance is required. Sureweld 6013 is recommended for welding vehicle bodies, profiles, tanks, ducts chassis, freight cars, ornamental jobs and thin-sheet structures.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Charpy V-Notch Properties

As Welded
Impact Value 35 ft-lb
Impact Value 47 J
Testing Temperature 32 °F
Testing Temperature 0 °C

Typical Tensile Properties

ConditionElongationReduction in AreaTensile Strength Yield Strength
As Welded27 %55 %558 MPa (81 ksi)482 MPa (70 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%)
120-135 A 1 kg/h (2.1 lb/h) 3.2 mm (1/8 in.) 73 %
60-90 A 0.7 kg/h (1.6 lb/h) 2.4 mm (3/32 in.) 73 %
145-190 A 1.2 kg/h (2.6 lb/h) 4.0 mm (5/32 in.) 75 %
145-190 A 1.45 kg/h (3 lb/h) 4.0 mm (5/32 in.) 74 %

Classifications

Grade E6013
Name AWS A5.1

Approvals

Grade E4913
Society CWB CSA W48
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Coating Type High titania
Welding Current DC+, DC- or AC

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Si
0.10 % 0.60 % 0.50 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 6013
812000152 FIND A DISTRIBUTOR
812000164 FIND A DISTRIBUTOR
812000156
812000145 FIND A DISTRIBUTOR
812000149
812000157 FIND A DISTRIBUTOR
812000172
812000181 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..