Sureweld 6011

ESAB

Sureweld 6011

The following items have been added to your list


x

Sureweld 6011 is an all-position, cellulosic type electrode designed for AC. It produces an easily controlled forceful arc with deep penetration and a high quality weld metal which will pass specification requirements for radiography. Sureweld 6011 is used primarily for welding mild steels such as ASTM A-36, A-283, A-284, A-285, A-515, A516 and ABS hull and boiler steel. Typical applications include welding of buildings, piping, shipbuilding, pressure vessels and tanks. AC-DCEP (Electrode Positive).

BUY NOW


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationReduction in AreaTensile Strength Yield Strength
As Welded22 %56 %524 MPa (76 ksi)462 MPa (67 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Optimal Amps
60-80 A 0.9 kg/h (2 lb/h) 2.4 mm (3/32 in.) 60 % 70 A
85-120 A 1.1 kg/h (2.4 lb/h) 3.2 mm (1/8 in.) 70 % 100 A
140-175 A 1.7 kg/h (3.7 lb/h) 4.0 mm (5/32 in.) 77 % 140 A
170-210 A 1.8 kg/h (4.1 lb/h) 5.0 mm (3/16 in.) 73 % 180 A

Classifications

Grade E6011
Name AWS A5.1

Consumable Characteristics

Coating Type High cellulose
0
Welding Current AC or DC+

Typical Weld Metal Analysis %

C Mn P S Si
0.10 % 0.36 % 0.012 % 0.012 % 0.15 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 6011
812000099
812000107
812000095 FIND A DISTRIBUTOR
812000131
812000073
812000081
812000069 FIND A DISTRIBUTOR
812000115
812000123

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..