Sureweld 6010 is an all-position, quick solidifying cellulosic type electrode with minimal spatter and excellent arc control. It offers deep penetration and easy removal of slag which allows single and multiple pass welds of x-ray quality. Sureweld 6010 adapts exceptionally well to vertical and overhead projects on all mild steels. Sureweld 6010 is used extensively in the welding of holding tanks, freight cars, and truck chassis.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Tensile Properties

ConditionElongationReduction in AreaShielding GasTensile Strength Yield Strength
As Welded28 %65 %100% CO2490 MPa (71 ksi)427 MPa (62 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%)
85-120 A 1.1 kg/h (2.4 lb/h) - 3.2 mm (1/8 in.) 63.9 % - -
170-210 A 1.7 kg/h (3.7 lb/h) - 5.0 mm (3/16 in.) 67 % - -
60-80 A 0.9 kg/h (2 lb/h) - 2.4 mm (3/32 in.) 60 % - -
140-175 A 1.4 kg/h (3 lb/h) - 4.0 mm (5/32 in.) 71.9 % - -

Classifications

Grade E6010
Name AWS A5.1

Approvals

Society ABS
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Coating Type High cellulose
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
0.10 % 0.36 % 0.01 % 0.01 % 0.20 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 6010
SW 6010 1/8X14X1# TUBE 812000020 FIND A DISTRIBUTOR
SW 6010 1/8X14X44#CTN 812000032 FIND A DISTRIBUTOR
SW 6010 1/8X14X5#VALP 812000024
SW 6010 3/16x14x44#CTN 812000065 FIND A DISTRIBUTOR
SW 6010 3/32X14X1# TUBE 812000004 FIND A DISTRIBUTOR
SW 6010 3/32X14X44#CTN 812000016 FIND A DISTRIBUTOR
SW 6010 3/32X14X5#VALP 812000008
SW 6010 5/32X14X44#CTN 812000057 FIND A DISTRIBUTOR
SW 6010 5/32X14X5#VALP 812000040
x
x

x

Loading..