Atom Arc 9018 electrodes are used for attachment welds on T-1, HY-80 and HY-90 steels and other high tensile, quenched and tempered steels.
Industries
- Bridge Construction
- Civil Construction
- Industrial and General Fabrication
- Mobile Equipment
- Railcars
- Ship/Barge Building
Welding Process
- SMAW/MMA (Stick)
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Mn | Mo | Ni | P | S | Si | ||||||||
0.043 % | 1.00 % | 0.29 % | 1.60 % | 0.012 % | 0.01 % | 0.26 % | ||||||||
0.012 % |