ATOM ARC 9018-CM

ATOM ARC 9018-CM

The principal application of Atom Arc 9018-CM electrodes is for welding 2 1/2% Cr - 1% Mo steels commonly found in pressure vessels, heat exchangers, pipings and other related components.

Where To Buy


Industries

  • Power Generation
  • Pipeline

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1275 °F 1 hr 102 ksi 85 ksi
Stress Relieved 26 % 1275 °F 8 hr 97 ksi 82 ksi
Stress Relieved 22 % 1275 °F 20 hr 100 ksi 85 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 97 ft-lb 1275 °F 8 hr 32 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnX-FactorMoCSSiCr
0.011 %0.70 %<15 %1.10 %0.07 %0.008 %0.40 %2.20 %

Approvals: ABS; AWS A5.5: E9018-B3; MIL-E-0022200/8; MIL-9018-B3
Classifications: ASME SFA 5.5; AWS A5.5; E9018-B3 H4R

Approvals are based on factory location. Please contact ESAB for more information.


Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1275 °F 1 hr 102 ksi 85 ksi
Stress Relieved 26 % 1275 °F 8 hr 97 ksi 82 ksi
Stress Relieved 22 % 1275 °F 20 hr 100 ksi 85 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 97 ft-lb 1275 °F 8 hr 32 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnX-FactorMoCSSiCr
0.011 %0.70 %<15 %1.10 %0.07 %0.008 %0.40 %2.20 %

Approvals: ABS; AWS A5.5: E9018-B3; MIL-E-0022200/8; MIL-9018-B3
Classifications: ASME SFA 5.5; AWS A5.5; E9018-B3 H4R

Approvals are based on factory location. Please contact ESAB for more information.


Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ATOM ARC 9018-CM
AA 9018-CM 5/32X14X50#HS 255075319 Buy Local
AA 9018-CM 5/32X14X10#HS 255075327 Buy Local
AA 9018-CM 3/32X14X50#HS 255073314 Buy Local
AA 9018-CM 3/32X14X10#HS 255073322 Buy Local
AA 9018-CM 1/8X14X10#HS 255071821 Buy Local
AA 9018-CM 1/8X14X50#HS 255071813 Buy Local
AA 9018-CM 3/16X14X50#HS 255073116 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..