Atom Arc 9018-B91 is designed to weld martensitic 95% Cr & 1% Mo-V steels known by the designations T91, P91 or Grade 91. These steels are designed to provide improved creep strength, fatigue, oxidation, and corrosion resistance at elevated temperatures. It also provides good weld metal ductility and high charpy values at room temperature. This product is optimized to meet the requirements for Mn + Ni contents < 1.0 wt %.

Where To Buy


Industries

  • Pipeline
  • Power Generation
  • Petrochemical

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 25 % 62 % 1400 °F 2 hr 106 ksi 86 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 69 ft-lb 1400 °F 2 hr 70 °F

Typical Weld Metal Analysis %

MnX-FactorMoCMn+NiNCrPCuSNbVSiNi
0.75 %<15 ppm %0.92 %0.10 %<1.0 %0.043 %8.48 %0.01 %0.04 %0.01 %0.04 %0.21 %0.20 %0.21 %

Classifications: AWS A5.5; : E9018-B91-H4R; ASME SFA 5.5

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 25 % 62 % 1400 °F 2 hr 106 ksi 86 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 69 ft-lb 1400 °F 2 hr 70 °F

Typical Weld Metal Analysis %

MnX-FactorMoCMn+NiNCrPCuSNbVSiNi
0.75 %<15 ppm %0.92 %0.10 %<1.0 %0.043 %8.48 %0.01 %0.04 %0.01 %0.04 %0.21 %0.20 %0.21 %

Classifications: AWS A5.5; : E9018-B91-H4R; ASME SFA 5.5

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Atom Arc 9018-B91
AA 9018-B91 3/32X14X10#HS XF 255067846 Buy Local
AA 9018-B91 5/32X14X10#HS XF 255067861 Buy Local
AA 9018-B91 1/8X14X10#HS XF 255067853 Buy Local