Atom Arc 8018
Atom Arc 8018 electrodes deposit 1% Ni weld metal. They are used primarily to weld high-tensile steels in the 70-80 ksi (483-552 MPa) tensile strength range, especially where notch toughness at temperatures as low as -40°F (-40°C) is required.
Industries
- Bridge Construction
- Industrial and General Fabrication
- Mobile Equipment
- Petrochemical
- Pipeline
- Power Generation
- Ship/Barge Building
Welding Process
- SMAW/MMA (Stick)
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Cu | Mn | Mo | Nb | Ni | P | S | Si | V | ||||
0.045 % | 0.06 % | 0.139 % | 1.08 % | 0.12 % | 0.003 % | 0.91 % | 0.01 % | 0.01 % | 0.31 % | 0.009 % |