ATOM ARC 8018-B8'

ESAB

ATOM ARC 8018-B8

ATOM ARC 8018-B8

Atom Arc 8018-B8 is designed to weld 9% Cr - 1% Mo creep resisting steels such as ASTM A213-T9 and A335-P9. These steels are used in pressure vessels and piping for high temperature service.

BUY NOW


Industries

  • Power Generation
  • Pipeline
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Testing Temperature Testing Time Yield Strength
Stress Relieved 22 % 98 ksi 1375 °F 1 hr 79 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoCSX-barSiCr
0.01 %0.80 %1.00 %0.07 %0.01 %< 15 ppm0.30 %8.60 %

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B8 H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Tensile Strength Testing Temperature Testing Time Yield Strength
Stress Relieved 22 % 98 ksi 1375 °F 1 hr 79 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoCSX-barSiCr
0.01 %0.80 %1.00 %0.07 %0.01 %< 15 ppm0.30 %8.60 %

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B8 H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ATOM ARC 8018-B8
AA 8018-B8 5/32X14X10#HS 255187924 FIND A DISTRIBUTOR
AA 8018-B8 1/8X14X10#HS 255187916 FIND A DISTRIBUTOR
AA 8018-B8 3/32X14X10#HS 255187908 FIND A DISTRIBUTOR
AA 8018-B8 3/16X14X10#HS 255187932 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..