ATOM ARC 8018-B6L

ATOM ARC 8018-B6L

Atom Arc 8018-B6L deposits a low carbon 5% Cr, 0.5% Mo weld metal. It is designed for welding ASTM A200-T5, A335-P5, A387-Gr5 and similar steels. Applications tend to be in the petrochemical and petroleum industries, especially where hydrogen attack accelerates metal failure. Additionally, these steels are used in pressure vessels and piping for high temperature service.

Where To Buy


Industries

  • Pipeline
  • Power Generation

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 25 % 1375 °F 1 hr 81 ksi 95 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSiNiCr
0.015 %0.60 %0.60 %0.04 %0.011 %0.60 %0.05 %5.40 %

Approvals: MIL-22200/8; MIL-E-502-15
Classifications: ASME SFA 5.5; AWS A5.5; E8018-B6L H4R

Approvals are based on factory location. Please contact ESAB for more information.


x

Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 25 % 1375 °F 1 hr 81 ksi 95 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSiNiCr
0.015 %0.60 %0.60 %0.04 %0.011 %0.60 %0.05 %5.40 %

Approvals: MIL-22200/8; MIL-E-502-15
Classifications: ASME SFA 5.5; AWS A5.5; E8018-B6L H4R

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ATOM ARC 8018-B6L
AA 8018-B6L 1/8X14X10#HS 255187817 Buy Local
AA 8018-B6L 3/32X14X10#HS 255187809 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..