ATOM ARC 8018-B6

ATOM ARC 8018-B6

Atom Arc 8018-B6 is designed to weld 5% Cr - 1/2% Mo creep resisting steels such as ASTM A387 Grade 5, A213-T5 and A335-P5. These steels are normally used in pressure vessels and piping for high temperature service.

Where To Buy


Industries

  • Power Generation
  • Pipeline
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1375 °F 1 hr 101 ksi 86 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoX-FactorCSSiCr
0.013 %0.70 %0.60 %< 15 %0.07 %0.009 %0.50 %5.30 %

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B6 H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 23 % 1375 °F 1 hr 101 ksi 86 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoX-FactorCSSiCr
0.013 %0.70 %0.60 %< 15 %0.07 %0.009 %0.50 %5.30 %

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B6 H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ATOM ARC 8018-B6
AA 8018-B6 5/32X14X10#HS 255197824 Buy Local
AA 8018-B6 3/32X14X10#HS 255197808 Buy Local
AA 8018-B6 1/8X14X10#HS 255197816 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..