Atom Arc 8018-B3L electrodes contain 2 1/4% Cr and 1% Mo alloy additions with low carbon content. The electrode is designed for welding 2 1/4% Cr - 1% Mo steels. The rod operates with a very stable arc and minimal spatter. The low carbon analysis of the weld metal contributes to its crack resistance. The addition of Cr and Mo provide for the excellent creep and stress rupture properties of weldments subjected to elevated temperature service.

BUY NOW


Industries

  • Mobile Equipment
  • Pipeline
  • Power Generation

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Testing Temperature Testing Time Yield Strength
Stress Relieved 25 % 93 ksi 1275 °F 1 hr 78 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoX-barCSSiCr
0.017 %0.70 %1.10 %<15 ppm0.04 %0.015 %0.40 %2.30 %

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B3L H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Tensile Strength Testing Temperature Testing Time Yield Strength
Stress Relieved 25 % 93 ksi 1275 °F 1 hr 78 ksi

Typical Weld Metal Analysis %

weld metal analysis
PMnMoX-barCSSiCr
0.017 %0.70 %1.10 %<15 ppm0.04 %0.015 %0.40 %2.30 %

Classifications: ASME SFA 5.5; AWS A5.5; E8018-B3L H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ATOM ARC 8018-B3L
AA 8018-B3L 3/32X14X10#HS 255173320 FIND A DISTRIBUTOR
AA 8018-B3L 3/32X14X50#HS 255173312 FIND A DISTRIBUTOR
AA 8018-B3L 5/32X14X10#HS 255175325 FIND A DISTRIBUTOR
AA 8018-B3L 1/8X14X10#HS 255171829 FIND A DISTRIBUTOR
AA 8018-B3L 1/8X14X50#HS 255171811 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..