Atom Arc 7018-Mo

ESAB

Atom Arc 7018-Mo

The following items have been added to your list


x

Atom Arc 7018-Mo electrodes contain 1/2% Mo as alloy addition. They are recommended for welding low-alloy, high tensile steels of 50 ksi (345 MPa) minimum yield strength and also 1/2% Molybdenum steels and pipes. They are widely employed in the fabrication and erection of boilers, pressure piping and tubing and other pressure vessel applications.

BUY NOW


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Power Generation

Welding Process

  • SMAW/MMA (Stick)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Mo P S Si
0.04 % 0.80 % 0.55 % 0.012 % 0.01 % 0.40 %
0.012 % 0.40 %

Approvals

Society ABS
Grade AWS A5.5: E7018-A1
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Classifications

Name ASME SFA 5.5
Grade E7018-A1 H4R
Name AWS A5.5

Consumable Characteristics

Welding Current AC or DC+
0
Coating Type Low-hydrogen iron powder

Typical Tensile Properties

Condition Stress Relieved Stress Relieved Stress Relieved As Welded
Tensile Strength (met) 607 MPa(88 ksi) 587 MPa(85 ksi) 607 MPa(88 ksi) 600 MPa(87 ksi)
Yield Strength (met) 524 MPa(76 ksi) 504 MPa(73 ksi) 518 MPa(75 ksi) 530 MPa(77 ksi)
Elongation 28 % 29 % 29 % 27 %
Testing Time 8 hr 20 hr 1 hr
Testing Temperature (met) 620 degC(1150 degF) 620 degC(1150 degF) 620 degC(1150 degF)

Deposition Data

Current Deposition Rate Diameter Efficiency (%) Optimal Amps
130-220 A 1.7 kg/h(3.8 lb/h) 4.0 mm(5/32 in.) 73.5 % 170 A
90-160 A 1.2 kg/h(2.6 lb/h) 3.2 mm(1/8 in.) 71.6 % 120 A
200-300 A 2.4 kg/h(5.4 lb/h) 4.8 mm(3/16 in.) 74.6 % 250 A
200-300 A 2.2 kg/h(4.9 lb/h) 4.8 mm(3/16 in.) 76.4 % 200 A
70-100 A 0.8 kg/h(1.7 lb/h) 2.4 mm(3/32 in.) 66.3 % 90 A
90-160 A 1.2 kg/h(2.7 lb/h) 3.2 mm(1/8 in.) 70.9 % 140 A
250-350 A 3.3 kg/h(7.2 lb/h) 5.6 mm(7/32 in.) 74 % 300 A
250-350 A 2.9 kg/h(6.5 lb/h) 5.6 mm(7/32 in.) 75 % 250 A
130-220 A 1.4 kg/h(3.1 lb/h) 4.0 mm(5/32 in.) 75 % 140 A
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Atom Arc 7018-Mo
AA 7018-MO 1/4X18X50#HS 255021412 FIND A DISTRIBUTOR
AA 7018-MO 1/8X14X10#HS 255021826 FIND A DISTRIBUTOR
AA 7018-MO 1/8X14X50#HS 255021818 FIND A DISTRIBUTOR
AA 7018-MO 3/16X14X50#HS 255023111 FIND A DISTRIBUTOR
AA 7018-MO 3/32X14X10#HS 255023327 FIND A DISTRIBUTOR
AA 7018-MO 3/32X14X50#HS 255023319 FIND A DISTRIBUTOR
AA 7018-MO 5/32X14X10#HS 255025322 FIND A DISTRIBUTOR
AA 7018-MO 5/32X14X50#HS 255025314 FIND A DISTRIBUTOR
AA 7018-MO 7/32X18X50#HS 255027310 FIND A DISTRIBUTOR