ATOM ARC 12018'

ESAB

ATOM ARC 12018

ATOM ARC 12018

Atom Arc 12018 is recommended for use in fabrication of low-alloy, high tensile steels where welds of 120 ksi (830 MPa) minimum tensile strength are required. Atom Arc 12018 is typically used to weld forging, casting plate and pressure vessels.

BUY NOW


Industries

  • Automotive
  • Industrial and General Fabrication
  • Railcars
  • Mobile Equipment

Welding Process

  • SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 18 % 56 % 133 ksi 120 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 26 ft-lb -60 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnCuMoCSNbVSiNiCr
0.01 %1.88 %0.092 %0.23 %0.047 %0.01 %0.005 %0.010 %0.35 %1.94 %0.63 %

Classifications: ASME SFA 5.5; AWS A5.5; E12018M H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 18 % 56 % 133 ksi 120 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 26 ft-lb -60 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnCuMoCSNbVSiNiCr
0.01 %1.88 %0.092 %0.23 %0.047 %0.01 %0.005 %0.010 %0.35 %1.94 %0.63 %

Classifications: ASME SFA 5.5; AWS A5.5; E12018M H4R

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : ATOM ARC 12018
AA 12018 3/16X14X50#HS 255103111 FIND A DISTRIBUTOR
AA 12018 1/8X14X50#HS 255101818 FIND A DISTRIBUTOR
AA 12018 3/32X14X50#HS 255107336 FIND A DISTRIBUTOR
AA 12018 5/32X14X50#HS 255105314 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..