Atom Arc 12018-M2

Atom Arc 12018-M2

Atom Arc 12018-M2 is a low hydrogen, iron powder all-position electrode specially formulated to meet the more stringent requirements of Military Specification MIL-E-0022200/10 for mechanical properties, low coating moisture and diffusible hydrogen content. Hydrogen coupons analyzed by the gas chromatography method showed an average of 0.026 ml/g of diffusible hydrogen. The average percent by weight of coating moisture is 0.07% when removed from a hermetically sealed can and 0.17% after 9 hours exposure at 80ºF (27ºC) and 80% relative humidity.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 21 % 64 % 118 ksi 109 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 75 ft-lb 0 °F
As Welded 60 ft-lb -60 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnCuMoSCNbVSiNiCr
0.01 %1.77 %0.032 %0.29 %0.01 %0.039 %0.004 %0.010 %0.27 %3.43 %0.03 %

Classifications: MIL; 12018M2

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+
x

Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 21 % 64 % 118 ksi 109 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 75 ft-lb 0 °F
As Welded 60 ft-lb -60 °F

Typical Weld Metal Analysis %

weld metal analysis
PMnCuMoSCNbVSiNiCr
0.01 %1.77 %0.032 %0.29 %0.01 %0.039 %0.004 %0.010 %0.27 %3.43 %0.03 %

Classifications: MIL; 12018M2

Coating Type: Low-hydrogen iron powder
CTOD-Tested: False
Welding Current: AC or DC+