Atom Arc 10018 electrodes are used primarily for applications which require weld joints of at least 100 ksi (690 MPa) tensile strength, good ductility and crack resistance. Good notch toughness at temperatures as low as -60°F (-51°C) is possible with this electrode. Atom Arc 10018 can be used to weld HY-80 and T-1 steel.

BUY NOW


Industries

  • Bridge Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn Mo Ni P S Si
0.051 % 1.46 % 0.27 % 1.72 % 0.013 % 0.011 % 0.31 %

Typical Charpy V-Notch Properties

Classifications

Name ASME SFA 5.5
Grade E10018M H4R
Name AWS A5.5

Consumable Characteristics

Welding Current AC or DC+
0
Coating Type Low-hydrogen iron powder

Typical Tensile Properties

ConditionElongationReduction in AreaTensile Strength (imp)Yield Strength (imp)
As Welded24 %64 %745 MPa (108 ksi)685 MPa (99 ksi)

Deposition Data

Current Deposition Rate Diameter Efficiency (%) Optimal Amps
90-160 A 1.2 kg/h(2.6 lb/h) 3.2 mm(1/8 in.) 71.6 % 120 A
90-160 A 1.2 kg/h(2.7 lb/h) 3.2 mm(1/8 in.) 70.9 % 140 A
130-220 A 1.7 kg/h(3.8 lb/h) 4.0 mm(5/32 in.) 73.5 % 170 A
200-300 A 2.2 kg/h(4.9 lb/h) 4.8 mm(3/16 in.) 76.4 % 200 A
200-300 A 2.4 kg/h(5.4 lb/h) 4.8 mm(3/16 in.) 74.6 % 250 A
130-220 A 1.1 kg/h(3.1 lb/h) 4.0 mm(5/32 in.) 75 % 140 A
70-100 A 0.8 kg/h(1.7 lb/h) 2.4 mm(3/32 in.) 66.3 % 170 A
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Atom Arc 10018
AA 10018 1/8X14X50#HS 255081812 FIND A DISTRIBUTOR
AA 10018 3/16X14X50#HS 255083115 FIND A DISTRIBUTOR
AA 10018 5/32X14X50#HS 255085318 FIND A DISTRIBUTOR
x
x

x

Loading..