Atom Arc 10018-MM
Atom Arc 10018-MM electrodes are used to weld low-alloy, high-tensile steels where welds of 100 ksi (690 MPa) minimum tensile strength is required. This electrode is recommended for use in the weld repair and fabrication of Mn-Mo steel castings and armor plate.
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Cu | Mn | Mo | Nb | Ni | P | S | Si | V | ||||
0.081 % | 0.17 % | 0.083 % | 1.93 % | 0.34 % | 0.004 % | 0.32 % | 0.01 % | 0.01 % | 0.33 % | 0.011 % |
Typical Charpy V-Notch Properties
Testing Temperature | -51 degC |
Testing Temperature | -60 degF |
1 hr | |
621 degC | |
1150 degF | |
Impact Value (met) | 33 J |
Impact Value (imp) | 24 ft-lb |
Stress Relieved |