Atom Arc 10018-M1 is a low hydrogen, iron powder all-position electrode specially formulated to meet the more stringent requirements of Military Specification MIL-E-0022200/10 for mechanical properties, low coating moisture and diffusible hydrogen content. Hydrogen coupons analyzed by the gas chromatography method showed an average of 0.03 ml/g of diffusible hydrogen.  Atom Arc 10018-M1 electrode is intended for welding high tensile steels, such as HY-80, HSLA-80, A710 and T-1 steel.

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Nb Ni P S Si V
0.040 % 0.04 % 0.037 % 1.52 % 0.29 % 0.004 % 2.27 % 0.01 % 0.01 % 0.35 % 0.011 %

Typical Charpy V-Notch Properties

Classifications

Name MIL
Grade 10018M1

Consumable Characteristics

Welding Current AC or DC+
0
Coating Type Low-hydrogen iron powder

Typical Tensile Properties

ConditionElongationReduction in AreaTensile Strength (imp)Yield Strength (imp)
As Welded24 %67 %672 MPa (97 ksi)617 MPa (90 ksi)