Sureweld 7018

ESAB

Sureweld 7018

The following items have been added to your list


x

Sureweld 7018 is a general purpose, easy-to-use basic DC+ electrode with good mechanical properties for welding of mild steels. Sureweld 7018 is an excellent all around performer with good welder appeal, covering many applications for mild and low alloy steels.

BUY NOW


Industries

  • Automotive
  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • SMAW/MMA (Stick)

Typical Charpy V-Notch Properties

As Welded
Impact Value 107 ft-lb
Impact Value 145 J
Testing Temperature -20 °F
Testing Temperature -29 °C

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded27 %607 MPa (88 ksi)538 MPa (78 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Optimal Amps
90-160 A 1.2 kg/h (2.6 lb/h) 3.2 mm (1/8 in.) 71.6 % 120 A
70-100 A 0.8 kg/h (1.7 lb/h) 2.4 mm (3/32 in.) 66.3 % 90 A
130-220 A 1.1 kg/h (3.1 lb/h) 4.0 mm (5/32 in.) 75 % 140 A

Classifications

Classifications ASME SFA 5.1 :
AWS A5.1 : E7018

Approvals

Society ABS
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Coating Type Low-hydrogen iron powder
0
Welding Current AC or DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Mn P S Si
0.04 % 1.33 % 0.012 % 0.005 % 0.58 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Sureweld 7018
812000308 FIND A DISTRIBUTOR
812000320 FIND A DISTRIBUTOR
812000312
812000301 FIND A DISTRIBUTOR
812000313 FIND A DISTRIBUTOR
812000305
812000332 FIND A DISTRIBUTOR
812000324